99.95% Pure Zirconium Sputtering Target and 705 702 Zirconium Plate
1.Zirconium 702 Wire
2.Commercially pure Zirconium 702 wire exhibits good ductility even at cryogenic temperatures.
3.Zirconium 702 Wire has good strength comparable with other common engineering alloys.
We strictly control the quality of products, all Titanium Target, Molydenum, Gr2 Welding Neck Flange have passed the quality supervision and inspection center inspection. We firmly believe that professionalism creates value and trust comes from responsibility. We have the courage to research innovative technology, continuous improvement, and get the praise of large enterprises. Facing the future, we are full of confidence, we win by virtue, we win by quality. In the silent search and cultivation of the road, we have had the opportunity to make numerous mentors and friends.
APPLICATIONS
Zirconium 702 wire used in Metal gaskets for chemical processing plants, Getter straps, Nuclear components
DESCRIPTION
Zirconium 702 exhibits good ductility in cryogenic temperatures. It has good strength Zirconium is a reactive metal ,It has a high affinity for oxygen resulting in the formation of a protective oxide layer in air at nomal room temperature. This protective oxide gives zirconium702 wire their superior corrosion resistance.
CHEMISTRY TYPICAL
| Zirconium + Hafnium | 99.2 min | Carbon: | 0.05 max | |
| Iron + Chromium | 0.2 max | Oxygen: | 0.16 min | |
| Hafnium | .5 max | Nitrogen | 0.025 max | |
| Hydrogen | 0.005 max |
PHYSICAL PROPERTIES
Density: 0.235 lbs/in3, 6.51 g/cm3
Mean Coefficient of Thermal Expansion: in/in/° F (µm/m/°C):
70 - 212 °F [20 - 100 ° C] 3.2 * 10-5 [5.8]
Thermal Conductivity: BTU-in/h-ft-° F (W/m-° K): 70 ° F (21 degree): 13 (22)
Modulus of Elasticity, ksi (mPa):
14.4 * 103 (99.2 * 103) in tension
5.25 *103 (36.2 *103) in shear
Fusion Point: 2550 degree F (1852 degree)
MECHANICAL PROPERTIES AT ROOM TEMPERATURE
ANNEALED TYPICAL
Tensile Strength: 55 KSI minium [379 MPa minium]
Yield Strength [0.2% offset]: 30 KSI minium [207 MPa minium]
Elongation: 16% minium
PROPERTIES TEMPERED
Zirconium 702 wire can be cold rolled ,Zirconium 702 wire can achieve the temper properties required according to specific customers and manufacturing requirements. Contact sales2@bjrcti.com
ADDITIONAL PROPERTIES
CORROSION RESISTANCE
Refer to NACE [National Associate of Corrosion Engineers] for suggestions
STANDARD WIRE FINISHES
Extra Clean: (XC) Extra clean is also call to "bright annealed" and " cold rolled".Also called bright annealed
Grease (only for round wire ): Using a heavy grease to produce an "Ultra bright" finish for the decorative applications
Soap (only using for round wire): Soap is used as a lubricant in the drawing process and is not need to removed. It can be use as a lubricant in customer part forming operation. A soap finish is valid in tempered products.
Plated: Many plating options are available.
*Special finishes are available: Contact sales2@bjrcti.com
We take excellent product quality of our 99.95% Pure Zirconium Sputtering Target and 705 702 Zirconium Plate, good reputation, and customer satisfaction as our success criteria. While the scale efficiency and influence of the enterprise are improved, we let the income of the employees grow simultaneously with the enterprise efficiency, and realize the common development of the employees and the enterprise. Corporate culture is the soul and commander of an enterprise. It is the foundation of an enterprise and the source of its vitality.
Hot Tags: zirconium 702 wire, suppliers, manufacturers, factory, customized, wholesale, bulk, pricelist, quotation, in stock, free sample, Titanium 180 Degree Elbow, Titanium Parts, Gr5 90 Degree Elbow, Molydenum, Titanium Coil Wire, Nickle
[[ProKeywords]]Send Inquiry