Pure Zirconium Sputtering Target Zr702 Zr704 Zr705 Zirconium
1.Zirconium 702 Wire
2.Commercially pure Zirconium 702 wire exhibits good ductility even at cryogenic temperatures.
3.Zirconium 702 Wire has good strength comparable with other common engineering alloys.
With the concept of 'customer satisfaction is the goal', we always take customer needs as the first to professionally develop and produce various Gr2 Welding Neck Flange, Titanium Spool Wire, Titanium Basket. In the face of the current competitive situation and market development, our company attaches importance to customer maintenance and retention, and constantly develops customers to meet the needs of sustainable, healthy and stable development of our company. Our company relies on the professional technical strength and advanced production equipment to produce high-quality products, and relies on price advantage, timely delivery and perfect service to win customers and the market. Quality is our life, reputation is our foundation, and service is our cornerstone!
APPLICATIONS
Zirconium 702 wire used in Metal gaskets for chemical processing plants, Getter straps, Nuclear components
DESCRIPTION
Zirconium 702 exhibits good ductility in cryogenic temperatures. It has good strength Zirconium is a reactive metal ,It has a high affinity for oxygen resulting in the formation of a protective oxide layer in air at nomal room temperature. This protective oxide gives zirconium702 wire their superior corrosion resistance.
CHEMISTRY TYPICAL
| Zirconium + Hafnium | 99.2 min | Carbon: | 0.05 max | |
| Iron + Chromium | 0.2 max | Oxygen: | 0.16 min | |
| Hafnium | .5 max | Nitrogen | 0.025 max | |
| Hydrogen | 0.005 max |
PHYSICAL PROPERTIES
Density: 0.235 lbs/in3, 6.51 g/cm3
Mean Coefficient of Thermal Expansion: in/in/° F (µm/m/°C):
70 - 212 °F [20 - 100 ° C] 3.2 * 10-5 [5.8]
Thermal Conductivity: BTU-in/h-ft-° F (W/m-° K): 70 ° F (21 degree): 13 (22)
Modulus of Elasticity, ksi (mPa):
14.4 * 103 (99.2 * 103) in tension
5.25 *103 (36.2 *103) in shear
Fusion Point: 2550 degree F (1852 degree)
MECHANICAL PROPERTIES AT ROOM TEMPERATURE
ANNEALED TYPICAL
Tensile Strength: 55 KSI minium [379 MPa minium]
Yield Strength [0.2% offset]: 30 KSI minium [207 MPa minium]
Elongation: 16% minium
PROPERTIES TEMPERED
Zirconium 702 wire can be cold rolled ,Zirconium 702 wire can achieve the temper properties required according to specific customers and manufacturing requirements. Contact sales2@bjrcti.com
ADDITIONAL PROPERTIES
CORROSION RESISTANCE
Refer to NACE [National Associate of Corrosion Engineers] for suggestions
STANDARD WIRE FINISHES
Extra Clean: (XC) Extra clean is also call to "bright annealed" and " cold rolled".Also called bright annealed
Grease (only for round wire ): Using a heavy grease to produce an "Ultra bright" finish for the decorative applications
Soap (only using for round wire): Soap is used as a lubricant in the drawing process and is not need to removed. It can be use as a lubricant in customer part forming operation. A soap finish is valid in tempered products.
Plated: Many plating options are available.
*Special finishes are available: Contact sales2@bjrcti.com
Facing the fast-paced technological innovation, diversified user needs, and increasingly fierce industry competition, our company constantly innovates and produces Pure Zirconium Sputtering Target Zr702 Zr704 Zr705 Zirconium that meet the market demand. In the process of development for many years, the company focuses on the creation of core products, increases investment in research and development, and vigorously explores the market. Our business model of integrating design, R&D and manufacturing enables us to provide total solutions for our customers, making product quality better and creating higher value for our customers.
Hot Tags: zirconium 702 wire, suppliers, manufacturers, factory, customized, wholesale, bulk, pricelist, quotation, in stock, free sample, Zirconium Tube, The Other Titanium Parts, Titanium Flange, titanium bolts metric, Molybdenum Bar, Titanium Target
[[ProKeywords]]Send Inquiry