R60702 Zirconium Tube for Sale Zirconium Target

R60702 Zirconium Tube for Sale Zirconium Target

1.Zirconium 702 Wire
2.Commercially pure Zirconium 702 wire exhibits good ductility even at cryogenic temperatures.
3.Zirconium 702 Wire has good strength comparable with other common engineering alloys.

Our company, as one of the leading manufacturers and exporters in the industry, is able to provide our customers with inexpensive and well-designed Zirconium Crucible, Gr2 Round Titanium Bar, Iridium Tantalum Titanium Anode. The products we produce have unique design, novel styles, scientific structure, low power consumption, high efficiency, good performance, and environmental protection. We keep pace with the times, forge ahead, and comprehensively promote the rapid and sustainable coordinated development of the enterprise. The quality management of modern enterprises needs the participation of all staff. It is not just a matter of one person, several quality management personnel or one department of the quality management department. It needs the close cooperation of all departments and the joint participation of all staff.

APPLICATIONS

Zirconium 702 wire used in Metal gaskets for chemical processing plants, Getter straps, Nuclear components

DESCRIPTION

 Zirconium 702 exhibits good ductility in cryogenic temperatures. It has good strength Zirconium is a reactive metal ,It  has a high affinity for oxygen resulting in the formation of a protective oxide layer in air at nomal room temperature. This protective oxide gives zirconium702 wire their superior corrosion resistance.


CHEMISTRY TYPICAL

Zirconium + Hafnium
99.2 min
Carbon:0.05 max
Iron + Chromium0.2 max
Oxygen: 0.16 min
Hafnium.5 max
Nitrogen0.025 max
Hydrogen0.005 max



PHYSICAL PROPERTIES


Density: 0.235 lbs/in3, 6.51 g/cm3

Mean Coefficient of Thermal Expansion:  in/in/° F (µm/m/°C):
70 - 212 °F [20 - 100 ° C] 3.2 * 10-5 [5.8]

Thermal Conductivity: BTU-in/h-ft-° F (W/m-° K): 70 ° F (21 degree): 13 (22)

Modulus of Elasticity, ksi (mPa):
14.4 * 103 (99.2 * 103) in tension
5.25 *103 (36.2 *103) in shear

Fusion Point: 2550 degree F (1852 degree)

MECHANICAL PROPERTIES AT ROOM TEMPERATURE

ANNEALED TYPICAL

Tensile Strength: 55 KSI minium [379 MPa minium]
Yield Strength [0.2% offset]: 30 KSI minium [207 MPa minium]
Elongation: 16% minium

PROPERTIES TEMPERED

Zirconium 702 wire can be cold rolled ,Zirconium 702 wire can achieve the temper properties required according to  specific customers and manufacturing requirements. Contact sales2@bjrcti.com

ADDITIONAL PROPERTIES

CORROSION RESISTANCE

Refer to NACE [National Associate of Corrosion Engineers] for suggestions

STANDARD WIRE FINISHES

Extra Clean: (XC) Extra clean is also call to  "bright annealed" and " cold rolled".Also called bright annealed 

Grease (only  for round wire ): Using a heavy grease to produce an "Ultra bright" finish for the decorative applications

Soap (only using for round wire): Soap is used as a lubricant in the drawing process and is not need to  removed. It can be use as a lubricant in customer part forming operation. A soap finish is valid in tempered products.

Plated: Many plating options are available.

*Special finishes are available: Contact sales2@bjrcti.com


In the continuous communication with users, we constantly optimize the humanized design, function and overall design of our R60702 Zirconium Tube for Sale Zirconium Target. We advocate the spirit of practical work, advocate the style of practical work, and pursue the culture of practical work. We rely on advanced equipment for a large number of technological innovations and continuous product development and production applications.

Hot Tags: zirconium 702 wire, suppliers, manufacturers, factory, customized, wholesale, bulk, pricelist, quotation, in stock, free sample, Tungstun, Nickle Bar, titanium anode plate for electrolysis, Gr5 90 Degree Elbow, motorcycle footpegs for sale, Titanium Anode Rod

[[ProKeywords]]

Send Inquiry